Nov 06, 2023 Lăsaţi un mesaj

Dimensiunile țevii din oțel inoxidabil ASTM A312

Țevi din oțel inoxidabil ASTM A312dimensiunile sunt stabilite de specificația ANSI ASME B36.19.

 

Greutatea conductei ASTM A312

Dimensiunea nominală a conductei Diametru exterior Dimensiuni țevi din oțel inoxidabil
Programul 5S Programul 10S Programul 40S Programul 80S
(mm) (inch) GREUTATE / GREUTATE
mm (inchi) kg/m mm (inchi) kg/m mm (inchi) kg/m mm (inchi) kg/m
1/8 10.3 0.405 – – 1.25 (0.049) 0.28 1.73 (0.068) 0.37 2.42 (0.095) 0.47
1/4 13.7 0.540 – – 1.66 (0.065) 0.49 2.24 (0.088) 0.63 3.03 (0.119) 0.80
3/8 17.2 0.675 – – 1.66 (0.065) 0.63 2.32 (0.091) 0.85 3.20 (0.126) 1.10
1/2 21.3 0.840 1.65 (0.065) 0.81 2.11 (0.083) 1.00 2.77 (0.109) 1.27 3.74 (0.147) 1.62
3/4 26.7 1.050 1.65 (0.065) 1.02 2.11 (0.083) 1.28 2.87 (0.113) 1.68 3.92 (0.154) 2.20
1 33.4 1.315 1.65 (0.065) 1.30 2.77 (0.109) 2.09 3.38 (0.133) 2.50 4.55(0.179) 3.24
1 1/4 42.2 1.660 1.65 (0.065) 1.66 2.77 (0.109) 2.69 3.56 (0.140) 3.39 4.86 (0.191) 4.47
1 1/2 48.3 1.900 1.65 (0.065) 1.91 2.77 (0.109) 3.11 3.69 (0.145) 4.06 5.08 (0.200) 5.41
2 60.3 2.375 1.65 (0.065) 2.40 2.77 (0.109) 3.93 3.92 (0.154) 5.45 5.54 (0.218) 7.49
2 1/2 73.0 2.875 2.11 (0.083) 3.69 3.05 (0.120) 5.26 5.16 (0.203) 8.64 7.01 (0.276) 11.4
3 88.9 3.500 2.11 (0.083) 4.52 3.05 (0.120) 6.46 5.49 (0.216) 11.3 7.62 (0.300) 15.3
3 1/2 101.6 4.000 2.11 (0.083) 5.18 3.05 (0.120) 7.41 5.74 (0.226) 13.6 8.08 (0.318) 18.6
4 114.3 4.500 2.11 (0.083) 5.84 3.05 (0.120) 8.37 6.02 (0.237) 16.1 8.56 (0.337) 22.3
5 141.3 5.563 2.77 (0.109) 9.46 3.41 (0.134) 11.6 6.56 (0.258) 21.8 9.53 (0.375) 31.0
6 168.3 6.625 2.77 (0.109) 11.3 3.41 (0.134) 13.9 7.12 (0.280) 28.3 10.9 (0.432) 42.6
8 219.1 8.625 2.77 (0.109) 14.8 3.76 (0.148) 20.0 8.18 (0.322) 42.5 12.7 (0.500) 64.6
10 273.1 10.750 3.41 (0.134) 22.7 4.20 (0.165) 27.8 9.28 (0.365) 60.4 12.7 (0.500) 81.5
12 323.9 12.750 3.97 (0.156) 31.3 4.58 (0.180) 36.1 9.53 (0.375) 73.9 12.7 (0.500) 97.4

 

Toleranța diametrului conductei ASTM A312

NPS Toleranță ASTM A312/ASME SA312 OD
+ –
inch mm inch mm
1/8 până la 1 1 /2
>1 1 /2 până la 4
>4 la 8
>8 până la 18
>18 până la 26
>26 până la 34
>34 până la 48
1/64(0.015)
1/32(0.031)
1/16(0.062)
3/32(0.093)
1/8(0.125)
5/32(0.156)
3/16(0.187)
0.4
0.8
1.6
2.4
3.2
4.0
4.8
1/32(0.031)
1/32(0.031)
1/32(0.031)
1/32(0.031)
1/32(0.031)
1/32(0.031)
1/32(0.031)
0.8
0.8
0.8
0.8
0.8
0.8
0.8

 

Toleranța la grosimea peretelui țevii ASTM A312

Toleranța nominală a grosimii peretelui este de +/- 12,5%.

NPS Toleranță ASTM A312/ASME SA312 WT, %
+ –
1/8-2 1 /2 20.0 12.5
3~18, t/D Mai mic sau egal cu 5% 22.5 12.5
3~18, t/D> 5% 15.0 12.5
Mai mare sau egal cu 20, sudate 17.5 12.5
Mai mare sau egal cu 20, fără sudură, t/D Mai mic sau egal cu 5% 22.5 12.5
≥ 20, seamless, t/D> 5% 15.0 12.5

 

 